Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.70 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
6.93 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Izod Impact, Notched | 3.70 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
6.93 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M5240 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 3.70 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
6.93 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding MR200 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 3.70 J/cm @Temperature -30.0 °C |
6.93 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Europe-Africa-Middle East) High flow PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 3.70 J/cm @Thickness 3.18 mm, Temperature -18.0 °C |
6.93 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ HTX M6307 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Izod Impact, Notched | 3.70 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
6.93 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Styron Pulse® B-270 PC/ABS Engineering ResinInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 3.70 J/cm @Temperature 23.0 °C |
6.93 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman DuraStar DS2000 Polymer, Natural Durastar DS2000 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2000 has ver.. |
|||
Izod Impact, Notched | 3.70 J/cm @Temperature 23.0 °C |
6.93 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman DuraStar DS2110UVI Polymer, Natural Durastar DS2110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Izod Impact, Notched | 3.70 J/cm @Temperature 23.0 °C |
6.93 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman DuraStar MN620 Polymer, Natural Applications:Blood therapyDrug deliveryIV componentsMedicalSurgical instrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAProduct Description: DuraStar Poly.. |
|||
Izod Impact, Notched | 3.70 J/cm @Temperature 23.0 °C |
6.93 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman DuraStar MN621 Polymer, Natural Durastar Polymer MN621 was developed for the medical device industry and contains a mold release It processes easily and requires minimal drying time. It has superior toughness, high clarity and goo.. |
|||
Izod Impact, Notched | 3.70 J/cm @Temperature 23.0 °C |
6.93 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar BR203 Copolyester Eastar BR203 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilitie.. |