Mechanical Properties Metric English Comments
Izod Impact, Notched 7.37 J/cm

@Temperature 23.0 °C
13.8 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® EXL1192C PC Copolymer
High flow, polycarbonate siloxane copolymer resin. Notched izod ductile to -20C ductility. Enhanced processability compared to standard PC resins. Available in a range of transparent colors. US ..