Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.48 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
14.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers PC/PBT-1420IM Polycarbonate+PBT, Superior Cold Temp Impact, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 7.48 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
14.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers PC/PBT-1422 Polycarbonate+PBT, Improved Cold Temp Impact, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |