Polymer Property : Izod Impact, Notched = 7.49 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.00 J/cm

@Temperature -30.0 °C
7.49 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Europe-Africa-Middle East)
UV stabilized, non-FR PC/ABS of excellent flow and impact performanceThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched 4.00 J/cm

@Temperature 23.0 °C
7.49 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP ..
Izod Impact, Notched 4.00 J/cm

@Thickness 3.17 mm
7.49 ft-lb/in

@Thickness 0.125 in
ASTM D256
PTS Trilac® ABS-HS7500 High Impact ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 4.00 J/cm

@Thickness 3.20 mm,
Temperature -32.0 °C
7.49 ft-lb/in

@Thickness 0.126 in,
Temperature -25.6 °F
ASTM D256
Kingfa MAC-851 PC/ABS Alloy
Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical ..
Izod Impact, Notched 4.00 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
7.49 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM-D256
Ineos ABS Lustran® 786 ABS, Extrusion Grade
Lustran® ABS 786 resin is a black, virgin extrusion grade of ABS (acrylonitrile butadiene styrene). It is designed for extruded drain, waste, and vent (DWV) pipe. Lustran® ABS 786 (901046 blac..
Izod Impact, Notched 4.00 J/cm

@Temperature 23.0 °C
7.49 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl EM6100F PPE+PS
Automotive interiors. 240F HDT. High impact/good property retention after heat ageing. In blowmolding, better sandability of flash, overblow.This data was supplied by SABIC-IP for the Americas re..
Izod Impact, Notched >= 4.00 J/cm

@Temperature 23.0 °C
>= 7.49 ft-lb/in

@Temperature 73.4 °F
Practical Use (Water Absorption 2.4%); ASTM-D256
Toyobo GLAMIDE® T-656E Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 4.00 J/cm

@Thickness 3.17 mm
7.49 ft-lb/in

@Thickness 0.125 in
TPI Porene® ABS-SP-100 Super High Impact ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 4.00 J/cm

@Temperature 23.0 °C
7.49 ft-lb/in

@Temperature 73.4 °F
Practical Use (Water Absorption 3.5%); ASTM-D256
Toyobo GLAMIDE® T-802 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 4.00 J/cm

@Temperature 23.0 °C
7.49 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Cossa Polimeri ESTADIENE 3008 MT Acrylonitrile Butadiene Styrene
ABS with very high impact resistanceHigh impact resistance at low temperature, medium heat resistance, good processabilityInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 4.00 J/cm

@Temperature 23.0 °C
7.49 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Cossa Polimeri ESTADIENE CR 1 Acrylonitrile Butadiene Styrene
ABS for chrome platingGood melt flow rate, high impact resistance at low temperature, high gloss, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched >= 4.00 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
>= 7.49 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256, ISO 180/4a
EPICHEM Epicarb PC Polycarbonate
Characteristics: high fluidity, good impact
Copyright © lookpolymers.com All Rights Reserved