Izod Impact, Notched 7.60 J/cm

@Temperature 23.0 °C
14.2 ft-lb/in

@Temperature 73.4 °F
3.2 mm (0.125 in) notch
Kraton® FG1901 + PBT blend (30/70), Oven Aged
Oven aged at 150°C (°F) for 2 hours. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A-B]n). The KRATON G series are second generation block polymers in whi..