Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.48 J/cm @Temperature 23.0 °C |
15.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SLX2531T PC Copolymer (Europe-Africa-Middle East) Transparent weatherable PC copolymer for blowmolding/extrusion.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |