Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.00 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
16.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L9630 Polyvinyl Chloride, Rigid (PVC, Rigid) Product can meet UL-94V-0. Material passed V-0 @ 1.5mm in screening test at PDI.Information provided by PolyOne |