Mechanical Properties Metric English Comments
Izod Impact, Notched 5.10 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
9.55 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Kingfa JH960 HT10 Non-halogenated Flame Retardant PC/ABS Alloy
Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc..
Izod Impact, Notched 5.10 J/cm

@Temperature -34.0 °C
9.55 ft-lb/in

@Temperature -29.2 °F
ASTM D256
Styron PULSEâ„¢ EXT 200 PC/ABS Engineering Resin
Overview: High Heat, High Impact PC/ABS resin for injection molded automotive plating and painting trim applications.Information provided by Styron