Mechanical Properties Metric English Comments
Izod Impact, Notched 5.23 J/cm

@Temperature 23.0 °C
9.80 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp..
Izod Impact, Notched 5.23 J/cm

@Temperature 23.0 °C
9.80 ft-lb/in

@Temperature 73.4 °F
3.2 mm (0.125 in) notch
Kraton® G1652 + PP blend + Talc (12/21/67)
Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the ..
Izod Impact, Notched 5.23 J/cm

@Temperature 23.0 °C
9.80 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tenite 307A4000018 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Izod Impact, Notched 5.23 J/cm

@Temperature 23.0 °C
9.80 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tenite 307E4000018 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Izod Impact, Notched 5.23 J/cm

@Temperature 23.0 °C
9.80 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tenite 380A3V32818 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Izod Impact, Notched 5.23 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
9.80 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Axiall 8264 Rigid PVC, Extrusion