Polymer Property : Modulus of Elasticity = 1100 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 7.58 GPa

@Thickness 1.57 mm
1100 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP320U Cotton Fabric
Description: Utility version of NP320E. Meets most, but not all, NEMA properties for L and LE, and is not certifiable as a NEMA Grade.Thickness Tested: 0.062", 0.125", and 0.500"
Modulus of Elasticity 7.58 GPa

@Thickness 1.57 mm
1100 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP322 Cotton Fabric
Description: Linen phenolic laminate with molybdenum disulfide. Provides the same lubricity as NP313, but has better machining qualities. Mechanical strength similar to, but slightly less than NP320..
Modulus of Elasticity 7.58 GPa

@Thickness 1.57 mm
1100 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP325 Cotton Fabric
Description: Linen phenolic laminate with graphite added as a solid lubricant. Linen substrate provides better machining and wear resistance than NP315.Thickness Tested: 0.062", 0.125" and 0.500".
Modulus of Elasticity 7.58 GPa

@Thickness 1.57 mm
1100 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP344 Cotton Fabric
Description: Fine weave canvas laminate with high temperature phenolic resin and molybdenum disulfide lubricant. Good machining properties and low coefficient of thermal expansion. Better machining ..
Modulus of Elasticity 7.58 GPa

@Thickness 1.57 mm
1100 ksi

@Thickness 0.0620 in
LW; ASTM D229
Industrial Laminates/Norplex NP318 Cotton Fabric
Description: Post-forming canvas phenolic material. Mechanical and electrical properties similar to NP310E. It is made from a cotton fabric weighing more than 4 ounces per square yard and having a t..