Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 134 GPa @Temperature 900 °C |
19400 ksi @Temperature 1650 °F |
|
Special Metals INCOLOY® alloy 864 INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma.. |