Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 140 GPa @Temperature 1000 °C |
20300 ksi @Temperature 1830 °F |
Dynamic |
Haynes 282® Nickel Alloy Autogenously Welded Sheet Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 140 GPa @Temperature 1000 °C |
20300 ksi @Temperature 1830 °F |
Dynamic |
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 140 GPa @Temperature 1000 °C |
20300 ksi @Temperature 1830 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 140 GPa @Temperature 1000 °C |
20300 ksi @Temperature 1830 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 140 GPa @Temperature 1000 °C |
20300 ksi @Temperature 1830 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 140 GPa @Temperature 1000 °C |
20300 ksi @Temperature 1830 °F |
Dynamic |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 140 GPa @Temperature 1000 °C |
20300 ksi @Temperature 1830 °F |
Dynamic |
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Modulus of Elasticity | 140 GPa @Temperature 1000 °C |
20300 ksi @Temperature 1830 °F |
Dynamic |
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C) Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas.. |
|||
Modulus of Elasticity | 140 GPa @Temperature 1000 °C |
20300 ksi @Temperature 1830 °F |
Dynamic |
Haynes 282® Nickel Alloy Sheet, Gamma-Prime Strengthened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |
|||
Modulus of Elasticity | 140 GPa @Temperature 1000 °C |
20300 ksi @Temperature 1830 °F |
Dynamic |
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |