Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 98.0 GPa @Temperature 20.0 °C |
>= 14200 ksi @Temperature 68.0 °F |
Condition T4 (Quenching in water at RT) |
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition T4 Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |