Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 168 GPa @Temperature 600 °C |
24400 ksi @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |