Polymer Property : Modulus of Elasticity = 175 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 175 GPa

@Temperature 700 °C
25400 ksi

@Temperature 1290 °F
Dynamic
Haynes 282® Nickel Alloy Autogenously Welded Sheet
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Modulus of Elasticity 175 GPa

@Temperature 700 °C
25400 ksi

@Temperature 1290 °F
Dynamic
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Modulus of Elasticity 175 GPa

@Temperature 700 °C
25400 ksi

@Temperature 1290 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Modulus of Elasticity 175 GPa

@Temperature 700 °C
25400 ksi

@Temperature 1290 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Modulus of Elasticity 175 GPa

@Temperature 700 °C
25400 ksi

@Temperature 1290 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Modulus of Elasticity 175 GPa

@Temperature 700 °C
25400 ksi

@Temperature 1290 °F
Dynamic
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Modulus of Elasticity 175 GPa

@Temperature 700 °C
25400 ksi

@Temperature 1290 °F
Dynamic
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Modulus of Elasticity 175 GPa

@Temperature 300 °C
25400 ksi

@Temperature 572 °F
Special Metals INCOLOY® alloy 864
INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma..
Modulus of Elasticity 175 GPa

@Temperature 700 °C
25400 ksi

@Temperature 1290 °F
Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy
INCONEL® alloy N06230 (UNS N06230 / W.Nr. 2.4733) is a carbide strengthened nickel-chromium-tungsten-molybdenum alloy with an exceptional combination of strength, stability, and resistance to cor..
Modulus of Elasticity 175 GPa

@Temperature 399 °C
25400 ksi

@Temperature 750 °F
EDRO UltraChem® #15 Precipitation Hardening Stainless Mold Steel
Ultrachem® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by: exceptional corrosion resistance, uniform hardness in all dimensions, ..
Modulus of Elasticity 175 GPa

@Temperature 399 °C
25400 ksi

@Temperature 750 °F
EDRO UltraChem® ESR #16 Precipitation Hardening Stainless Mold Steel
Ultrachem ESR® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by exceptional polishability, exceptional corrosion resistance, unifor..
Modulus of Elasticity 175 GPa

@Temperature 700 °C
25400 ksi

@Temperature 1290 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Gamma-Prime Strengthened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..
Modulus of Elasticity 175 GPa

@Temperature 700 °C
25400 ksi

@Temperature 1290 °F
Dynamic
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..