Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 128.7 GPa @Temperature 927 °C |
18670 ksi @Temperature 1700 °F |
|
Special Metals INCONEL® alloy 783 Ni-Co-Fe Alloy The newest of the high-performance superalloys invented by Special Metals Corporation, INCONEL® alloy 783 (UNS R30783/US Patent 5,478,417), is an oxidation-resistant, low expansion, nickel-cobalt.. |