Polymer Property : Modulus of Elasticity = 21520 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 148.4 GPa

@Temperature 200 °C
21520 ksi

@Temperature 392 °F
Special Metals INCOLOY® Alloy 903
A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a..