Mechanical Properties Metric English Comments
Modulus of Elasticity 218 GPa

@Temperature 27.0 °C
31600 ksi

@Temperature 80.6 °F
Haynes R-41 alloy,
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Modulus of Elasticity 218 GPa

@Temperature 25.0 °C
31600 ksi

@Temperature 77.0 °F
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F)
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Modulus of Elasticity 218 GPa

@Temperature 21.0 °C
31600 ksi

@Temperature 69.8 °F
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F)
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Modulus of Elasticity 218 GPa

@Temperature 21.0 °C
31600 ksi

@Temperature 69.8 °F
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1121°C, air cooled, aged 16 hours at 899°C
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Modulus of Elasticity 218 GPa

@Temperature 100 °C
31600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 218 GPa

@Temperature 100 °C
31600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 218 GPa

@Temperature 100 °C
31600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 218 GPa

@Temperature 100 °C
31600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 218 GPa

@Temperature 100 °C
31600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 218 GPa

@Temperature 100 °C
31600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 218 GPa

@Temperature 100 °C
31600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 218 GPa

@Temperature 100 °C
31600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 218 GPa

@Temperature 100 °C
31600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Modulus of Elasticity 218 GPa

@Temperature 100 °C
31600 ksi

@Temperature 212 °F
Special Metals INCONEL® alloy 740 Precipitation-Hardenable Ni-Cr-Co Superalloy
INCONEL® alloy 740 is a nickel-chromium-cobalt alloy developed by Special Metals Corporation. The alloy is age hardenable by the precipitation of a gamma prime second phase. Potential applicati..
Modulus of Elasticity 218 GPa

@Temperature 20.0 °C
31600 ksi

@Temperature 68.0 °F
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel
BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303..
Modulus of Elasticity 218 GPa

@Temperature 100 °C
31600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl..
Modulus of Elasticity 218 GPa

@Temperature 100 °C
31600 ksi

@Temperature 212 °F
Dynamic
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl..
Modulus of Elasticity 218 GPa

@Temperature 27.0 °C
31600 ksi

@Temperature 80.6 °F
Haynes R-41 alloy,
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications include ..