Polymer Property : Modulus of Elasticity = 231 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 231 GPa

@Temperature 100 °C
33500 ksi

@Temperature 212 °F
Typical annealed sample; short time elevated temp.
American Utility Metals Cromgard® Stainless Steel
Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o..