Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 23900 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 165 GPa

@Temperature 800 °C
23900 ksi

@Temperature 1470 °F
Dynamic
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750)
Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for..
Modulus of Elasticity 165 GPa

@Temperature 800 °C
23900 ksi

@Temperature 1470 °F
Dynamic
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C)
Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas..
Modulus of Elasticity 165 GPa

@Temperature 500 °C
23900 ksi

@Temperature 932 °F
Special Metals INCONEL® alloy 693
INCONEL alloy 693 is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to t..
Modulus of Elasticity 165 GPa

@Temperature 600 °C
23900 ksi

@Temperature 1110 °F
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel
A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re..
Modulus of Elasticity 165 GPa

@Temperature 600 °C
23900 ksi

@Temperature 1110 °F
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel
Description: Hot work tool steel featuring excellent hot tensile properties, high retention of hardness, good toughness and resistance to heat checking, admits water cooling. BOHLER W303 is also ava..
Modulus of Elasticity 165 GPa

@Temperature 600 °C
23900 ksi

@Temperature 1110 °F
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel
W400 VMR is a low silicon, chromium-vanadium hot work tool steel which has been vacuum remelted to obtain the highest uniformity, the best cleanliness of tool steel. The material is characterized:E..
Modulus of Elasticity 165 GPa

@Temperature 600 °C
23900 ksi

@Temperature 1110 °F
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel
W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to ..
Modulus of Elasticity 165 GPa

@Temperature 649 °C
23900 ksi

@Temperature 1200 °F
Carpenter Thermo-Span® Fe-Co-Ni Superalloy
Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h..
Modulus of Elasticity 165 GPa

@Temperature 600 °C
23900 ksi

@Temperature 1110 °F
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel
Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits wat..