Mechanical Properties Metric English Comments
Modulus of Elasticity 183 GPa

@Temperature 427 °C
26500 ksi

@Temperature 801 °F
Dynamic
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Modulus of Elasticity 183 GPa

@Temperature 427 °C
26500 ksi

@Temperature 801 °F
Dynamic
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Modulus of Elasticity 183 GPa

@Temperature 600 °C
26500 ksi

@Temperature 1110 °F
Dynamic
Haynes 282® Nickel Alloy Autogenously Welded Sheet
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Modulus of Elasticity 183 GPa

@Temperature 600 °C
26500 ksi

@Temperature 1110 °F
Dynamic
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Modulus of Elasticity 183 GPa

@Temperature 600 °C
26500 ksi

@Temperature 1110 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Modulus of Elasticity 183 GPa

@Temperature 600 °C
26500 ksi

@Temperature 1110 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Age-hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Modulus of Elasticity 183 GPa

@Temperature 600 °C
26500 ksi

@Temperature 1110 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Modulus of Elasticity 183 GPa

@Temperature 600 °C
26500 ksi

@Temperature 1110 °F
Dynamic
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Modulus of Elasticity 183 GPa

@Temperature 600 °C
26500 ksi

@Temperature 1110 °F
Dynamic
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la..
Modulus of Elasticity 183 GPa

@Temperature 427 °C
26500 ksi

@Temperature 801 °F
Dynamic
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Modulus of Elasticity 183 GPa

@Temperature 427 °C
26500 ksi

@Temperature 801 °F
Dynamic
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Modulus of Elasticity 183 GPa

@Temperature 600 °C
26500 ksi

@Temperature 1110 °F
Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy
INCONEL® alloy N06230 (UNS N06230 / W.Nr. 2.4733) is a carbide strengthened nickel-chromium-tungsten-molybdenum alloy with an exceptional combination of strength, stability, and resistance to cor..
Modulus of Elasticity 183 GPa

@Temperature 600 °C
26500 ksi

@Temperature 1110 °F
Dynamic
Haynes 282® Nickel Alloy Sheet, Gamma-Prime Strengthened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..
Modulus of Elasticity 183 GPa

@Temperature 427 °C
26500 ksi

@Temperature 801 °F
Dynamic
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..
Modulus of Elasticity 183 GPa

@Temperature 427 °C
26500 ksi

@Temperature 801 °F
Dynamic
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..
Modulus of Elasticity 183 GPa

@Temperature 600 °C
26500 ksi

@Temperature 1110 °F
Dynamic
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..
Modulus of Elasticity 183 GPa

@Temperature 427 °C
26500 ksi

@Temperature 801 °F
Dynamic
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..
Copyright © lookpolymers.com All Rights Reserved