Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 195 GPa @Temperature 500 °C |
28300 ksi @Temperature 932 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 195 GPa @Temperature 500 °C |
28300 ksi @Temperature 932 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 195 GPa @Temperature 500 °C |
28300 ksi @Temperature 932 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 195 GPa @Temperature 500 °C |
28300 ksi @Temperature 932 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 195 GPa @Temperature 500 °C |
28300 ksi @Temperature 932 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 195 GPa @Temperature 500 °C |
28300 ksi @Temperature 932 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 195 GPa @Temperature 500 °C |
28300 ksi @Temperature 932 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 195 GPa @Temperature 500 °C |
28300 ksi @Temperature 932 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 195 GPa @Temperature 500 °C |
28300 ksi @Temperature 932 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Modulus of Elasticity | 195 GPa @Temperature 20.0 °C |
28300 ksi @Temperature 68.0 °F |
|
Special Metals INCOLOY® alloy 864 INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma.. |
|||
Modulus of Elasticity | 195.1 GPa @Temperature 22.0 °C |
28300 ksi @Temperature 71.6 °F |
|
Special Metals INCOLOY® alloy 890 Ni-Cr-Fe Superalloy INCOLOY® alloy 890 (UNS N08890) is the latest addition to the INCOLOY alloy family of heat resistant alloys. Alloy 890 joins the existing INCOLOY products in offering high strength along with ex.. |
|||
Modulus of Elasticity | 195 GPa @Temperature 500 °C |
28300 ksi @Temperature 932 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
Modulus of Elasticity | 195 GPa @Temperature 500 °C |
28300 ksi @Temperature 932 °F |
Dynamic |
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
Modulus of Elasticity | 195 GPa @Temperature 300 °C |
28300 ksi @Temperature 572 °F |
|
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium .. |