Mechanical Properties Metric English Comments
Modulus of Elasticity 199 GPa

@Temperature 200 °C
28900 ksi

@Temperature 392 °F
Dynamic
Haynes 625SQ® Nickel Alloy Sheet
Haynes 625SQ alloy is a solid-solution strengthened superalloy. It is a modification of Haynes 625 alloy designed to enhance resistance to fatigue at temperatures up to approximately 1200°F (649Â..
Modulus of Elasticity 199 GPa

@Temperature 300 °C
28900 ksi

@Temperature 572 °F
Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy
INCONEL® alloy N06230 (UNS N06230 / W.Nr. 2.4733) is a carbide strengthened nickel-chromium-tungsten-molybdenum alloy with an exceptional combination of strength, stability, and resistance to cor..