Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 203 GPa @Temperature 200 °C |
29400 ksi @Temperature 392 °F |
|
Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy INCONEL® alloy N06230 (UNS N06230 / W.Nr. 2.4733) is a carbide strengthened nickel-chromium-tungsten-molybdenum alloy with an exceptional combination of strength, stability, and resistance to cor.. |