Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 2.50 GPa @Temperature 60.0 °C |
363 ksi @Temperature 140 °F |
ISO 527 |
BASF Ultrason E 3010 PES Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance. |