Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.30 GPa @Temperature 23.0 °C |
624 ksi @Temperature 73.4 °F |
TD; Test speed 1%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2 |
Mitsubishi Hostaphan® RN, 190 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin.. |
|||
Modulus of Elasticity | 4.30 GPa @Temperature 23.0 °C |
624 ksi @Temperature 73.4 °F |
TD; Test speed 1%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2 |
Mitsubishi Hostaphan® RN, 250 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin.. |
|||
Modulus of Elasticity | 4.30 GPa @Temperature 23.0 °C |
624 ksi @Temperature 73.4 °F |
TD; Test speed 1%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2 |
Mitsubishi Hostaphan® RN, 350 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties.Applications:Films for industrial applicationsCoatingLamin.. |