Mechanical Properties Metric English Comments
Modulus of Elasticity 6.21 GPa

@Thickness 1.57 mm
900 ksi

@Thickness 0.0620 in
LW; ASTM D229
Industrial Laminates/Norplex NP159 Synthetic Fabric  (discontinued **)
Description: Woven aramid fiber fabric combined with high temperature phenolic resin. With a proper post baking procedure, NP159 will withstand continuous operation at 200° C. Material becomes brit..
Modulus of Elasticity 6.21 GPa

@Thickness 1.57 mm
900 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP842 Paper Base Laminate  (discontinued **)
Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP842 is semi-conductive on the surfaces and through the laminate.Thickness Tested: 0..
Modulus of Elasticity 6.21 GPa

@Thickness 1.57 mm
900 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP611 Paper Base Laminate
Description: Hot punching general-purpose phenolic grade. Mechanical properties approach those of NP610 with improved electrical properties and moisture resistance.Thickness Tested: 0.062", 0 125" a..
Modulus of Elasticity 6.21 GPa

@Thickness 1.57 mm
900 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP680 Paper Base Laminate
Description: Hot punching grade with electrical properties between NP611 to NP631.Thickness Tested: 0.062", 0.125" & 0.500"
Modulus of Elasticity 6.21 GPa

@Thickness 1.57 mm
900 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP691 Paper Base Laminate
Description: Flame resistant, room temperature punching grade. NP691 is very similar to NP612 in electrical properties and mechanical strength, with improved moisture resistance.Thickness Tested: 0...
Modulus of Elasticity 6.21 GPa

@Thickness 1.57 mm
900 ksi

@Thickness 0.0620 in
LW; ASTM D229
Industrial Laminates/Norplex NP310U Cotton Fabric
Description: Utility grade canvas phenolic with properties similar to NP310E.Not certifiable to NEMA due to low crosswise flexural strength. Previously designated NP310C.Thickness Tested: 0.062", 0...
Modulus of Elasticity 6.21 GPa

@Thickness 1.57 mm
900 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP318 Cotton Fabric
Description: Post-forming canvas phenolic material. Mechanical and electrical properties similar to NP310E. It is made from a cotton fabric weighing more than 4 ounces per square yard and having a t..