Polymer Property : Modulus of Elasticity = 6000 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 41.4 GPa

@Thickness 1.57 mm
6000 ksi

@Thickness 0.0620 in
LW; ASTM D229
Industrial Laminates/Norplex NP545 Carbon Fiber  (discontinued **)
Description: NP545 is composed of carbon fiber fabric and an epoxy resin system. It has excellent moisture resistance and physical properties. Potential uses include fixtures and gage systems, high ..