Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | >= 68.0 GPa @Temperature 200 °C |
>= 9860 ksi @Temperature 392 °F |
|
PEAK Werkstoff DISPAL S250 Aluminum Alloy, AlSi20Fe5Ni2, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |