Mechanical Properties Metric English Comments
Modulus of Elasticity 5.00 GPa

@Temperature 23.0 °C
725 ksi

@Temperature 73.4 °F
TD; Test speed 1%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2
Mitsubishi Hostaphan® RN, 12 micron Nominal Thickness Universal Polyethylene Terephthalate Film
Hostaphan® RN is a transparent, biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties. Hostaphan® RN is the standard product for..
Modulus of Elasticity 5.00 GPa

@Temperature 23.0 °C
725 ksi

@Temperature 73.4 °F
TD; Test speed 1%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2
Mitsubishi Hostaphan® RN, 15 micron Nominal Thickness Universal Polyethylene Terephthalate Film
Hostaphan® RN is a transparent, biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties. Hostaphan® RN is the standard product for..
Modulus of Elasticity 5.00 GPa

@Temperature 23.0 °C
725 ksi

@Temperature 73.4 °F
TD; Test speed 1%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2
Mitsubishi Hostaphan® RN, 19 micron Nominal Thickness Universal Polyethylene Terephthalate Film
Hostaphan® RN is a transparent, biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties. Hostaphan® RN is the standard product for..
Modulus of Elasticity 5.00 GPa

@Temperature 23.0 °C
725 ksi

@Temperature 73.4 °F
TD; Test speed 1%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2
Mitsubishi Hostaphan® RN, 23 micron Nominal Thickness Universal Polyethylene Terephthalate Film
Hostaphan® RN is a transparent, biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties. Hostaphan® RN is the standard product for..
Modulus of Elasticity 5.00 GPa

@Temperature 23.0 °C
725 ksi

@Temperature 73.4 °F
TD; Test speed 1%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2
Mitsubishi Hostaphan® RN, 30 micron Nominal Thickness Universal Polyethylene Terephthalate Film
Hostaphan® RN is a transparent, biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties. Hostaphan® RN is the standard product for..