Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 5.52 GPa @Thickness 1.57 mm |
800 ksi @Thickness 0.0620 in |
CW; ASTM D229 |
Industrial Laminates/Norplex NP321 Cotton Fabric
(discontinued **) Description: NP321 consists of a fine weave cotton fabric (linen) impregnated with a phenolic resin binder. Applications include vanes for air and liquid pumps, and compressors. NP321 remains very f.. |