Mechanical Properties Metric English Comments
Tensile Stress 9.65 MPa

@Strain 300 %
1400 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® F7890 TPE, Fire Retardant
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsSealsWire & Cable ElectronicsInformation from Alliance Polymers & Services, Distributor of Nantong Elastome..
Tensile Stress 9.65 MPa

@Strain 100 %
1400 psi

@Strain 100 %
ASTM D412
Teknor Apex Telcar® TL-90-T707E-100 BLK 111 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Stress 9.67 MPa

@Strain 122.92 %,
Temperature 100 °C
1400 psi

@Strain 122.92 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 9.64 MPa

@Strain 0.180 %,
Temperature 150 °C
1400 psi

@Strain 0.180 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 92G35DH2 BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G35DH2 BK083 is a 35% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e..
Tensile Stress 9.68 MPa

@Strain 0.0900 %,
Temperature 0.000 °C
1400 psi

@Strain 0.0900 %,
Temperature 32.0 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66  (Unverified Data**)
Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in..
Tensile Stress 9.64 MPa

@Strain 0.220 %,
Temperature 150 °C
1400 psi

@Strain 0.220 %,
Temperature 302 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6  (Unverified Data**)
Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc..
Tensile Stress 9.66 MPa

@Strain 0.130 %,
Temperature 150 °C
1400 psi

@Strain 0.130 %,
Temperature 302 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..
Tensile Stress 9.63 MPa

@Strain 15.15 %,
Temperature 150 °C
1400 psi

@Strain 15.15 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1010 NC010 Nylon 1010  (Unverified Data**)
Unreinforced Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. ..
Tensile Stress 9.66 MPa

@Strain 45.0 %,
Temperature 80.0 °C
1400 psi

@Strain 45.0 %,
Temperature 176 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 9.64 MPa

@Strain 15.8 %,
Temperature 0.000 °C
1400 psi

@Strain 15.8 %,
Temperature 32.0 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 9.67 MPa

@Strain 0.530 %,
Temperature 120 °C
1400 psi

@Strain 0.530 %,
Temperature 248 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT  (Unverified Data**)
Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis..