Polymer Property : Tensile Stress = 0.150 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 0.150 MPa

@Strain 100 %
21.8 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® C4907 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 0.150 MPa

@Strain 0.000 %,
Temperature 175 °C
21.8 psi

@Strain 0.000 %,
Temperature 347 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FR52G30NH BK337 Polyphthalamide (PPA)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It..
Tensile Stress 0.150 MPa

@Strain 0.000 %,
Temperature -40.0 °C
21.8 psi

@Strain 0.000 %,
Temperature -40.0 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010  (Unverified Data**)
Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s..