Polymer Property : Tensile Stress = 0.621 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 0.621 MPa

@Strain 100 %,
Temperature 23.0 °C
90.1 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G2706-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G2706-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA and medical compliance. - High Puncture Reseal - Overmold Adhesion to Po..