Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.970 MPa @Strain 0.240 %, Temperature 90.0 °C |
141 psi @Strain 0.240 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610
(Unverified Data**) Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by.. |
|||
Tensile Stress | 0.970 MPa @Strain 0.120 %, Temperature 0.000 °C |
141 psi @Strain 0.120 %, Temperature 32.0 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |