Polymer Property : Tensile Stress = 1.40 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 1.40 MPa

@Strain 100 %
203 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® A9855A TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Tensile Stress 1.40 MPa

@Strain 300 %
203 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P3925T TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.40 MPa

@Strain 82.8 %,
Temperature 120 °C
203 psi

@Strain 82.8 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b..
Tensile Stress 1.40 MPa

@Strain 149.63 %,
Temperature 120 °C
203 psi

@Strain 149.63 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b..
Tensile Stress 1.40 MPa

@Strain 168.19 %,
Temperature 120 °C
203 psi

@Strain 168.19 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b..
Tensile Stress 1.40 MPa

@Strain 7.05 %,
Temperature 120 °C
203 psi

@Strain 7.05 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 1.40 MPa

@Strain 82.8 %,
Temperature 120 °C
203 psi

@Strain 82.8 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 1.40 MPa

@Strain 168.19 %,
Temperature 120 °C
203 psi

@Strain 168.19 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 1.40 MPa

@Strain 149.63 %,
Temperature 120 °C
203 psi

@Strain 149.63 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 1.40 MPa

@Strain 6.99 %,
Temperature 120 °C
203 psi

@Strain 6.99 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers