Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 10.02 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 10.02 MPa

@Strain 1.38 %,
Temperature 40.0 °C
1453 psi

@Strain 1.38 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo..
Tensile Stress 10.02 MPa

@Strain 0.190 %,
Temperature 200 °C
1453 psi

@Strain 0.190 %,
Temperature 392 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..
Tensile Stress 10.02 MPa

@Strain 75.29 %,
Temperature 90.0 °C
1453 psi

@Strain 75.29 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..