Polymer Property : Tensile Stress = 10.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 10.8 MPa

@Strain 1.10 %,
Temperature 90.0 °C
1570 psi

@Strain 1.10 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani..
Tensile Stress 10.8 MPa

@Strain 1.10 %,
Temperature 90.0 °C
1570 psi

@Strain 1.10 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b..
Tensile Stress 10.8 MPa

@Strain 132.12 %,
Temperature 120 °C
1570 psi

@Strain 132.12 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET
55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Stress 10.8 MPa

@Strain 300 %
1570 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G40D-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G40D-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 10.8 MPa

@Strain 300 %
1570 psi

@Strain 300 %
ISO 37
Alliance Polymers Viprene™ G40D-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G40D-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Copyright © lookpolymers.com All Rights Reserved