Tensile Stress 100.88 MPa

@Strain 1.16 %,
Temperature 40.0 °C
14631 psi

@Strain 1.16 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612  (Unverified Data**)
43% Glass Reinforced Polyamide 612Zytel 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers