Polymer Property : Tensile Stress = 102.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 102.3 MPa

@Strain 4.70 %,
Temperature -40.0 °C
14840 psi

@Strain 4.70 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 311DP BK402 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP BK402 is a medium high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced..