Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 70.55 MPa @Strain 3.31 %, Temperature -20.0 °C |
10230 psi @Strain 3.31 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 70.55 MPa @Strain 3.31 %, Temperature -20.0 °C |
10230 psi @Strain 3.31 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for .. |
|||
Tensile Stress | 70.53 MPa @Strain 0.900 %, Temperature 0.000 °C |
10230 psi @Strain 0.900 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |