Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 70.76 MPa @Strain 1.14 %, Temperature 23.0 °C |
10260 psi @Strain 1.14 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66
(Unverified Data**) 20% Glass Reinforced Heat Stabilized Polyamide 66 Developed for Blow Molding Zytel BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Perf.. |
|||
Tensile Stress | 70.74 MPa @Strain 1.36 %, Temperature 40.0 °C |
10260 psi @Strain 1.36 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G15HSLR BK031 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR BK031 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |