Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.10 MPa @Strain 300 % |
1030 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® F02-081A-10C TPE, Halogen Free Extrusion Grade Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to.. |
|||
Tensile Stress | 7.10 MPa @Strain 100 %, Temperature 21.0 °C |
1030 psi @Strain 100 %, Temperature 69.8 °F |
Across Flow 2 hr; ASTM D412 |
PolyOne Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Tensile Stress | 7.10 MPa @Strain 300 % |
1030 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3675 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 7.10 MPa @Strain 300 % |
1030 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3885H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 7.13 MPa @Strain 198.69 %, Temperature 120 °C |
1030 psi @Strain 198.69 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.12 MPa @Strain 98.26 %, Temperature 120 °C |
1030 psi @Strain 98.26 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.12 MPa @Strain 97.2 %, Temperature 120 °C |
1030 psi @Strain 97.2 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.12 MPa @Strain 98.26 %, Temperature 120 °C |
1030 psi @Strain 98.26 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.12 MPa @Strain 130.82 %, Temperature 150 °C |
1030 psi @Strain 130.82 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.10 MPa @Strain 0.200 %, Temperature 40.0 °C |
1030 psi @Strain 0.200 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.13 MPa @Strain 0.0600 %, Temperature -20.0 °C |
1030 psi @Strain 0.0600 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)
(Unverified Data**) 60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo.. |
|||
Tensile Stress | 7.13 MPa @Strain 0.0500 %, Temperature 40.0 °C |
1030 psi @Strain 0.0500 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |
|||
Tensile Stress | 7.10 MPa @Strain 48.0 %, Temperature 150 °C |
1030 psi @Strain 48.0 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.11 MPa @Strain 0.180 %, Temperature 180 °C |
1030 psi @Strain 0.180 %, Temperature 356 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66
(Unverified Data**) Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in.. |
|||
Tensile Stress | 7.09 MPa @Strain 0.300 %, Temperature -20.0 °C |
1030 psi @Strain 0.300 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie.. |
|||
Tensile Stress | 7.09 MPa @Strain 1.78 %, Temperature 40.0 °C |
1030 psi @Strain 1.78 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.09 MPa @Strain 7.59 %, Temperature 90.0 °C |
1030 psi @Strain 7.59 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC4601 NC010 Nylon
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide Developed for Extrusion Zytel RS LC4601 NC010 is a flexible toughened and plasticized polyamide resin intended for extrusion applications.Informatio.. |
|||
Tensile Stress | 7.10 MPa @Strain 0.500 %, Temperature 90.0 °C |
1030 psi @Strain 0.500 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Tensile Stress | 7.11 MPa @Strain 133.72 %, Temperature 120 °C |
1030 psi @Strain 133.72 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**) 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc.. |
|||
Tensile Stress | 7.08 MPa @Strain 145.72 %, Temperature 120 °C |
1030 psi @Strain 145.72 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin.. |
|||
Tensile Stress | 7.08 MPa @Strain 15.55 %, Temperature 40.0 °C |
1030 psi @Strain 15.55 %, Temperature 104 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.09 MPa @Strain 60.93 %, Temperature 90.0 °C |
1030 psi @Strain 60.93 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.10 MPa @Strain 300 % |
1030 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G85A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G85A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 7.10 MPa @Strain 300 % |
1030 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G85A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G85A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |