Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 7.412 MPa

@Strain 50.0 %
1075 psi

@Strain 50.0 %
Average; ASTM D412 Method A
Seals Eastern 7265 Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Vito..