Polymer Property : Tensile Stress = 11.34 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 11.34 MPa

@Strain 26.58 %,
Temperature 120 °C
1645 psi

@Strain 26.58 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers
Tensile Stress 11.34 MPa

@Strain 0.300 %,
Temperature -40.0 °C
1645 psi

@Strain 0.300 %,
Temperature -40.0 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D..
Tensile Stress 11.34 MPa

@Strain 0.0800 %,
Temperature -20.0 °C
1645 psi

@Strain 0.0800 %,
Temperature -4.00 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..