Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 11.9 MPa @Strain 300 %, Temperature 23.0 °C |
1730 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ CL E95 Thermoplastic Elastomer (TPE) Versaflex™ CL E95 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E95 is also formulated without the use of plasticizer.. |
|||
Tensile Stress | 11.9 MPa @Strain 50.0 % |
1720 psi @Strain 50.0 % |
ASTM D1708 |
DSM Biomedical Elasthane™ 55D Thermoplastic Polyether Polyurethane (TPU) A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility
Elasthane™ TPU exhibits outstanding hydrolytic stabilit.. |
|||
Tensile Stress | 11.9 MPa @Strain 0.300 %, Temperature 0.000 °C |
1730 psi @Strain 0.300 %, Temperature 32.0 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66
(Unverified Data**) Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP.. |
|||
Tensile Stress | 11.9 MPa @Strain 50.0 % |
1730 psi @Strain 50.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8341G BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Slightly Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 11.9 MPa @Strain 10.0 % |
1730 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |