Tensile Stress 12.8 MPa

@Strain 100 %
1860 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3895 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 12.8 MPa

@Strain 0.940 %,
Temperature 150 °C
1860 psi

@Strain 0.940 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal..
Tensile Stress 12.8 MPa

@Strain 240.5 %,
Temperature 150 °C
1860 psi

@Strain 240.5 %,
Temperature 302 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers