Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 83.1 MPa @Strain 9.10 %, Temperature -20.0 °C |
12100 psi @Strain 9.10 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem.. |
|||
Tensile Stress | 83.7 MPa @Strain 7.00 %, Temperature 0.000 °C |
12100 psi @Strain 7.00 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Tensile Stress | 83.7 MPa @Strain 8.00 %, Temperature 0.000 °C |
12100 psi @Strain 8.00 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Tensile Stress | 83.4 MPa @Strain 2.48 %, Temperature 23.0 °C |
12100 psi @Strain 2.48 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |
|||
Tensile Stress | 83.7 MPa @Strain 0.660 %, Temperature 40.0 °C |
12100 psi @Strain 0.660 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G45L NC010 Nylon 6
(Unverified Data**) 45% Glass Reinforced Polyamide 6Zytel 73G45L NC010 is a 45% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |