Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 84.94 MPa @Strain 1.56 %, Temperature 60.0 °C |
12320 psi @Strain 1.56 %, Temperature 140 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK609 NC010 PBT
(Unverified Data**) Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 84.93 MPa @Strain 2.57 %, Temperature -20.0 °C |
12320 psi @Strain 2.57 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |