Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 85.29 MPa @Strain 2.35 %, Temperature 0.000 °C |
12370 psi @Strain 2.35 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G15L NC010 Nylon 6
(Unverified Data**) 15% Glass Reinforced Polyamide 6Zytel 73G15L NC010 is a 15% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 85.27 MPa @Strain 4.35 %, Temperature -20.0 °C |
12370 psi @Strain 4.35 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie.. |
|||
Tensile Stress | 85.28 MPa @Strain 1.61 %, Temperature 23.0 °C |
12370 psi @Strain 1.61 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610
(Unverified Data**) 20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers |